METHODS FOR FORMING VERTICALLY CRACKED THERMAL BARRIER COATINGS AND ARTICLES INCLUDING VERTICALLY CRACKED THERMAL BARRIER COATINGS
PROBLEM TO BE SOLVED: To form a vertically cracked thermal barrier coating.SOLUTION: A vertically cracked thermal barrier coating (200) is formed by positioning an article (100) relative to a heat source (102). The article (100) includes a thermal barrier coating (202) disposed on a first surface (2...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
14.06.2018
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To form a vertically cracked thermal barrier coating.SOLUTION: A vertically cracked thermal barrier coating (200) is formed by positioning an article (100) relative to a heat source (102). The article (100) includes a thermal barrier coating (202) disposed on a first surface (204) of a substrate (206), and the substrate (206) includes a second surface (208) distal across the substrate (206) from the first surface (204). Heat is applied locally to a discrete portion (210) of the second surface (208) of the substrate (206). A vertical crack (212) in the thermal barrier coating (202) is formed over the discrete portion (210).SELECTED DRAWING: Figure 1
【課題】垂直亀裂遮熱コーティングを形成する。【解決手段】物品(100)を熱源(102)に対して位置決めし、垂直亀裂遮熱コーティング(200)を形成する。物品(100)は、基材(206)の第1の表面(204)上に配置された遮熱コーティング(202)を含み、基材(206)は、第1の表面(204)から基材(206)を越えて遠位の第2の表面(208)を含む。熱は、基材(206)の第2の表面(208)の不連続部分(210)に局所的に加えられる。遮熱コーティング(202)の垂直亀裂(212)は、不連続部分(210)の上に形成される。【選択図】図1 |
---|---|