BATTERY MANUFACTURING METHOD

PROBLEM TO BE SOLVED: To provide a battery manufacturing method capable of shortening a time period from the end of an initial charging process to the measurement of an IV resistance value Ra and appropriately measuring the IV resistance value Ra.SOLUTION: A manufacturing method of a battery 1 inclu...

Full description

Saved in:
Bibliographic Details
Main Authors IKEDA HIROAKI, SHIMURA YOSUKE, OTOMO TAKUYA, SUMI TOMOHIDE
Format Patent
LanguageEnglish
Japanese
Published 24.05.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a battery manufacturing method capable of shortening a time period from the end of an initial charging process to the measurement of an IV resistance value Ra and appropriately measuring the IV resistance value Ra.SOLUTION: A manufacturing method of a battery 1 includes an initial charging step S2 of initially charging the battery 1 up to a first battery voltage V1, a discharging step S3 of discharging the battery 1 up to a second battery voltage V2 after the initial charging step S2, a recharging step S4 of recharging the battery 1 up to a third battery voltage V3 lower than the first battery voltage V1 (V2<V3<V1) after the discharging step S3, and an IV resistance inspection step S5 of obtaining an IV resistance value Ra of the battery 1 after the recharging step S4 and determining whether the battery 1 is good or bad on the basis of the IV resistance value Ra.SELECTED DRAWING: Figure 5 【課題】初充電工程の終了時からIV抵抗値Raを測定するまでの期間を短くできると共に、IV抵抗値Raを適切に測定できる電池の製造方法を提供すること。【解決手段】電池1の製造方法は、電池1を第1電池電圧V1まで初充電する初充電工程S2と、初充電工程S2の後、電池1を第2電池電圧V2まで放電させる放電工程S3と、放電工程S3の後、電池1を第1電池電圧V1よりも低い第3電池電圧V3(V2<V3<V1)まで再充電する再充電工程S4と、再充電工程S4の後、電池1のIV抵抗値Raを取得し、このIV抵抗値Raに基づいて、当該電池1の良否を判定するIV抵抗検査工程S5とを備える。【選択図】図5
Bibliography:Application Number: JP20160223305