METHOD FOR PRODUCING BROWNMILLERITE OXIDES
PROBLEM TO BE SOLVED: To provide a method capable of producing brownmillerite oxides with quality uniformity and efficiency.SOLUTION: There is provided a method for producing brownmillerite oxides that employs, as raw materials, two or more kinds of solid compounds containing components that are of...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
10.05.2018
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide a method capable of producing brownmillerite oxides with quality uniformity and efficiency.SOLUTION: There is provided a method for producing brownmillerite oxides that employs, as raw materials, two or more kinds of solid compounds containing components that are of the composition of the target brownmillerite oxide. The method comprises a step A of mixing together two or more kinds of solid compounds serving as raw materials; a step B of griding the mixed raw material undergoing the step A to ensure that the mixed raw material is finely ground, preferably having a median particle size of 0.8 μm or less; and a step C of calcining the finely-ground mixed raw material obtained in the step B at a solid phase state. The calcining of the finely-ground mixed raw material at a solid phase state enables a molecular level contact to be sufficient for reaction. This allows an entirety of the mixed raw material to undergo a proper synthesis reaction. As a result, brownmillerite oxides with uniform quality are obtained.SELECTED DRAWING: Figure 1
【課題】ブラウンミラーライト型酸化物を品質にバラツキを生じることなく効率的に製造することができる製造方法を提供する。【解決手段】製造しようとするブラウンミラーライト型酸化物の組成の各成分をそれぞれ含む2種以上の固体化合物を原料としてブラウンミラーライト型酸化物を製造する方法であり、原料である2種以上の固体化合物を混合する工程Aと、この工程Aを経た混合原料を微粉状に粉砕、好ましくはメジアン粒径0.8μm以下に粉砕する工程Bと、この工程Bで得られた微粉状の混合原料を固相状態で焼成する工程Cを有する。微粉状の混合原料を固相状態で焼成することにより、分子レベルの接触が反応に十分な状態となるため、混合原料全体で合成反応が適切に生じ、均一な品質のブラウンミラーライト型酸化物が得られる。【選択図】図1 |
---|---|
Bibliography: | Application Number: JP20160209477 |