COPPER FOIL SHOWING SLACK RESISTANCE

PROBLEM TO BE SOLVED: To provide copper foil showing marvelous deformation resistance (e.g. slack resistance, sagging resistance, and wrinkle resistance).SOLUTION: Copper foil has a glossy surface of which the surface roughness (Rz) falls in a range of 0.6-1.9 μm, and a rough surface of which the su...

Full description

Saved in:
Bibliographic Details
Main Authors LIU YUEH-MIN, LAI YAO-SHENG, SHU ZUISHO, CHENG KUEI-SEN
Format Patent
LanguageEnglish
Japanese
Published 25.01.2018
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide copper foil showing marvelous deformation resistance (e.g. slack resistance, sagging resistance, and wrinkle resistance).SOLUTION: Copper foil has a glossy surface of which the surface roughness (Rz) falls in a range of 0.6-1.9 μm, and a rough surface of which the surface roughness (Rz) falls in a range of 0.6-1.9 μm. In addition, the copper foil has a color value Lvalue of the rough surface which is within a range of 12-35 according to Labcolor system, and a tensile strength of 34.1 kg/mmor less. A negative electrode comprises a negative electrode current collector having a negative electrode active material, in which the negative electrode current collector includes the copper foil. The negative electrode is applied to a lithium ion secondary battery.SELECTED DRAWING: Figure 7 【課題】驚異的な耐変形性(たとえば、耐たるみ性、耐垂れ性、および耐しわ性)を表す銅箔の提供。【解決手段】表面粗度(Rz)が0.6〜1.9μmの範囲にある光沢面、表面粗度(Rz)が0.6〜1.9μmの範囲にある粗面、L*a*b*表色系に準じて、12〜35の範囲にある粗面の明度L*値、および引張強度が34.1kg/mm2以下である銅箔。更に、負極集電体に負極活物質を有する負極であって、前記負極集電体が前記銅箔を含む、負極。前記負極を適用するリチウムイオン二次電池。【選択図】図7
Bibliography:Application Number: JP20170151508