PC/ABS COMPOSITIONS THAT RETAIN STABLE STATE DURING PROCESSING

PROBLEM TO BE SOLVED: To provide polycarbonate/ABS molding compositions which have improved stress cracking resistance and more stable high gloss and also exhibit lower thermal polycarbonate degradation under disadvantageous processing conditions (high temperature, high shear and/or long dwell time)...

Full description

Saved in:
Bibliographic Details
Main Authors SEIDEL ANDREAS, ECKEL THOMAS, MARTIN HAEUSLER
Format Patent
LanguageEnglish
Japanese
Published 21.12.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide polycarbonate/ABS molding compositions which have improved stress cracking resistance and more stable high gloss and also exhibit lower thermal polycarbonate degradation under disadvantageous processing conditions (high temperature, high shear and/or long dwell time) and a reduced content of free bisphenol A.SOLUTION: A thermoplastic molding composition comprises: A) 40.0 to 99.5 parts by weight of at least one aromatic polycarbonate or polyester carbonate having an OH end group content less than 300 ppm; B) 0.5 to 60.0 parts by weight of at least one graft polymer comprising lithium, sodium, potassium, magnesium and calcium of less than 100 ppm in total; C) 0.0 to 30.0 parts by weight of vinyl (co)polymer; and D) 0.0 to 40.0 parts by weight of other general polymer additives; where the sum of the parts by weight of components A) to D) is 100 parts by weight.SELECTED DRAWING: None 【課題】改善された耐応力亀裂性とより安定な高光沢を有し、又、不利な加工条件(高温、高剪断及び/又は長滞留時間)下でのより少ないポリカーボネート熱分解、及び遊離ビスフェノールAの低含量ポリカーボネート/ABS成形用組成物の提供。【解決手段】A)40.0〜99.5重量部の、OH末端基含量300ppm未満を有する少なくとも1種の芳香族ポリカーボネートまたはポリエステルカーボネート、B)0.5〜60.0重量部の、リチウム、ナトリウム、カリウム、マグネシウム及びカルシウムの総含量100ppm未満を有する少なくとも1種のグラフトポリマー、C)0.0〜30.0重量部のビニル(コ)ポリマー、D)0.0〜40.0重量部の他の一般的なポリマー添加剤を、成分A)〜D)の重量部の合計が100重量部となるように含んでなる熱可塑性成形用組成物。【選択図】なし
Bibliography:Application Number: JP20170138469