CIRCULAR GLASS SHEET AND PRODUCTION METHO THEREOF

PROBLEM TO BE SOLVED: To improve strength by reducing fine flaws or micro-cracks at a notched part on an outer peripheral edge of a circular glass sheet.SOLUTION: In a production method of a circular glass sheet, the circular glass sheet is produced from an original circular glass sheet 1 having a n...

Full description

Saved in:
Bibliographic Details
Main Authors ODANI OSAMU, IKEMOTO MASAYUKI
Format Patent
LanguageEnglish
Japanese
Published 02.11.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To improve strength by reducing fine flaws or micro-cracks at a notched part on an outer peripheral edge of a circular glass sheet.SOLUTION: In a production method of a circular glass sheet, the circular glass sheet is produced from an original circular glass sheet 1 having a notched part 2 and an un-notched part 3 where a notched part 2 is not formed, on an outer peripheral edge 4. The production method of the circular glass sheet has a processing step for heating the notched part 2 and the un-notched part 3 to above the softening point by scanning laser along the outer peripheral edge 4.SELECTED DRAWING: Figure 1 【課題】円形状のガラス板の外周縁の切り欠き部において、微小な傷やマイクロクラックを減少させることにより、強度を向上させる。【解決手段】本発明の円形状ガラス板の製造方法は、切り欠き部2と、切り欠き部2が形成されていない非切り欠き部3とを外周縁4に備えた円形状の元ガラス板1から円形状ガラス板を製造する。そして、本発明の円形状ガラス板の製造方法は、外周縁4に沿ってレーザを走査することにより、切り欠き部2及び非切り欠き部3を軟化点以上に加熱する加工工程を有する。【選択図】図1
Bibliography:Application Number: JP20160090618