THERMAL SHRINKABLE TUBE, ELECTRONIC COMPONENT OR BATTERY COATED WITH THE TUBE

PROBLEM TO BE SOLVED: To provide a thermal shrinkable tube having heat resistance without generating waviness of a tube or adhesion of a coated body even exposed to high temperature and excellent in impact resistance in a wide range temperature and mechanical strength.SOLUTION: There is provided a t...

Full description

Saved in:
Bibliographic Details
Main Author IKEDA KEITA
Format Patent
LanguageEnglish
Japanese
Published 03.08.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a thermal shrinkable tube having heat resistance without generating waviness of a tube or adhesion of a coated body even exposed to high temperature and excellent in impact resistance in a wide range temperature and mechanical strength.SOLUTION: There is provided a thermal shrinkable tube consisting of a polyester resin composition which contains 50 mass% or more and 95 mass% or less of a polyester resin (A) having 1,4-cyclohexanedimethanol of 5 to 50 mol% as a diol component, 5 mass% or more and less than 18 mass% of a polyamide resin (B) and 0 mass% or more and less than 20 mass% of a thermoplastic elastomer resin (C) and has tear strength measured in a length direction from a tube pleat as an origin by a trouser tearing method according to JIS K7128-1 of 80 N/cm or more.SELECTED DRAWING: None 【課題】高温下に曝されてもチューブの波打ちや被覆体の密着が起こらない耐熱性を有し、また、広い温度範囲での耐衝撃性や、機械的強度などに優れた熱収縮性チューブを提供する。【解決手段】ポリエステル系樹脂組成物からなる熱収縮性チューブであって、前記ポリエステル系樹脂組成物は、ジオール成分として、1,4−シクロヘキサンジメタノールを5〜50モル%含有するポリエステル系樹脂(A)50質量%以上95質量%以下、ポリアミド系樹脂(B)5質量%以上18質量%未満、及び熱可塑性エラストマー樹脂(C)0質量%以上20質量%未満含有し、JIS K7128−1に準拠し、トラウザー引裂法によりチューブ折目を起点として長さ方向に測定された引裂強度が80N/cm以上であることを特徴とする熱収縮性チューブ。【選択図】なし
Bibliography:Application Number: JP20160012947