COMPOSITE MOIRE FINISHED YARN AND MANUFACTURING METHOD THEREOF

PROBLEM TO BE SOLVED: To provide a composite moire finished yarn, which can express unique texture with natural tone of color and appearance, fullness, repulsive feeling and drape property of top moire and a manufacturing method of the composite moire finished yarn.SOLUTION: A composite moire finish...

Full description

Saved in:
Bibliographic Details
Main Authors KISHIDA YASUO, OBAYASHI TETSUHARU
Format Patent
LanguageEnglish
Japanese
Published 20.04.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a composite moire finished yarn, which can express unique texture with natural tone of color and appearance, fullness, repulsive feeling and drape property of top moire and a manufacturing method of the composite moire finished yarn.SOLUTION: A composite moire finished yarn is a combined filament entangled yarn including a cationic dye dyeable crimped filament yarn with 1 to 8 decitex single fiber fineness and a cationic dye non-dyeable side-by-side type crimped filament yarn with 2 to 6 decitex single fiber fineness. Occupancy of the cationic dye dyeable crimped filament yarn in the combined filament entangled yarn is 50 to 70%, number of interlacing is 100 to 180 count/m and crimping rate is 3 to 10%.SELECTED DRAWING: Figure 1 【課題】トップ杢調のナチュラルな色合い外観及びふくらみ感と反発感やドレープ性のある独特な風合いを表現する事ができる複合杢加工糸及びその製造方法を提供することを技術的な課題とするものである。【解決手段】単繊維繊度が1〜8dtexのカチオン染料可染性捲縮フィラメント糸と,単繊維繊度が2〜6dtexのカチオン染料不染性のサイドバイサイド型捲縮フィラメント糸を含む混繊交絡糸であって、該混繊交絡糸のカチオン染料可染性捲縮フィラメント糸の占有率が50〜70%であり、交絡数が100〜180個/mであり、捲縮率が3〜10%である複合杢加工糸。【選択図】図1
Bibliography:Application Number: JP20150202471