METHOD FOR MANUFACTURING NEGATIVE ELECTRODE FOR NONAQUEOUS ELECTROLYTE SECONDARY BATTERY

PROBLEM TO BE SOLVED: To provide a means capable of sufficiently reducing an amount of generated gas during initial charging in a nonaqueous electrolyte secondary battery.SOLUTION: A method for manufacturing a negative electrode for a nonaqueous electrolyte secondary battery of the present invention...

Full description

Saved in:
Bibliographic Details
Main Authors SHIMAMURA OSAMU, HAGIYAMA KOSUKE, MIYAMOTO KENJI, ICHIKAWA YOSHIHIRO, SATO MASANOBU
Format Patent
LanguageEnglish
Japanese
Published 09.02.2017
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a means capable of sufficiently reducing an amount of generated gas during initial charging in a nonaqueous electrolyte secondary battery.SOLUTION: A method for manufacturing a negative electrode for a nonaqueous electrolyte secondary battery of the present invention includes a step 1: a step of removing moisture in CMC (salt), and a step 2: coating an aqueous slurry on a collector and drying the slurry to form a negative electrode, the aqueous slurry containing a negative electrode active material, CMC (salt) obtained during the step 1, and an aqueous binder.SELECTED DRAWING: None 【課題】非水電解質二次電池において、初期充電時のガス発生量を十分に低減できる手段を提供することを目的とする。【解決手段】本発明の非水電解質二次電池用負極の製造方法は、工程1:CMC(塩)の水分を除去する工程と、工程2:集電体上に負極活物質、工程1で得られたCMC(塩)及び水系バインダを含む水系スラリを塗布、乾燥させて負極を形成する工程と、を含むことを特徴とする。【選択図】なし
Bibliography:Application Number: JP20150152839