ACTIVE CARBON MOLDED BODY AND MANUFACTURING METHOD THEREOF, AND ADSORBENT AND STORAGE MATERIAL THEREWITH
PROBLEM TO BE SOLVED: To provide active carbon molded body having enough strength, large specific surface area and large pore volume, and a manufacturing method thereof.SOLUTION: Active carbon molded body is provided by mixing active carbon with polyolefin resin which mean particle size is 1-50 μm,...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
12.01.2017
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide active carbon molded body having enough strength, large specific surface area and large pore volume, and a manufacturing method thereof.SOLUTION: Active carbon molded body is provided by mixing active carbon with polyolefin resin which mean particle size is 1-50 μm, and performing isotropy pressure treatment of the provided mixture.SELECTED DRAWING: Figure 1
【課題】十分な強度を有し、比表面積と細孔容積が大きい活性炭成形体、およびその製造方法を提供すること。【解決手段】本発明の活性炭成形体は、活性炭と平均粒子径1μm以上、50μm以下のポリオレフィン樹脂を混合し、得られた混合物を等方性加圧処理することによって得られることに要旨を有する。【選択図】図1 |
---|---|