METHOD FOR PRODUCING ANISOTROPIC MAGNET RIBBON
PROBLEM TO BE SOLVED: To provide a method for producing an anisotropic magnet ribbon capable of crystallizing an amorphous ribbon and capable of orienting an axis of easy magnetization in a direction vertical to a ribbon surface.SOLUTION: In a method for producing an anisotropic magnet ribbon, an am...
Saved in:
Main Authors | , , , , , , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
01.09.2016
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide a method for producing an anisotropic magnet ribbon capable of crystallizing an amorphous ribbon and capable of orienting an axis of easy magnetization in a direction vertical to a ribbon surface.SOLUTION: In a method for producing an anisotropic magnet ribbon, an amorphous ribbon is irradiated with a microwave to be heated to 550-850°C, the amorphous ribbon having a composition represented by: RFeCoBM(where R represents one or more selected from rare earth elements, M represents one or more selected from among Ga, Al, Cu, Au, Ag, Zn, In and Mn and inevitable impurity elements, and 5≤x≤20, 0≤y≤8, 4≤w≤6.5 and 0≤z≤2 are satisfied).SELECTED DRAWING: Figure 1
【課題】アモルファス薄帯を結晶化させると同時に、磁化容易軸を薄帯の面に垂直な方向に配向させることができる、異方性磁石薄帯の製造方法を提供する。【解決手段】RxFe100−x−y−w−zCoyBwMz(Rは希土類元素から選ばれる1種以上、MはGa、Al、Cu、Au、Ag、Zn、In及びMnから選ばれる1種以上と不可避的不純物元素、5≦x≦20、0≦y≦8、4≦w≦6.5、並びに0≦z≦2)で表される組織を有するアモルファス薄帯にマイクロ波を照射し、前記アモルファス薄帯を550〜850℃に加熱する。【選択図】図1 |
---|---|
Bibliography: | Application Number: JP20150034366 |