COMPOSITION FOR NON-ROTARY COATING, AND METHOD FOR FORMING RESIN COMPOSITION FILM

PROBLEM TO BE SOLVED: To provide a composition for non-rotary coating having excellent conformal properties; and to provide a method for forming a resin composition film using the composition for non-rotary coating.SOLUTION: A composition for non-rotary coating contains a resin (A) and a solvent (S)...

Full description

Saved in:
Bibliographic Details
Main Authors OUCHI YASUHIDE, KIKUCHI HIROYUKI, SAIJO HIDEKI, SOMEYA KAZUYA, HIKITA JIRO
Format Patent
LanguageEnglish
Japanese
Published 01.09.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a composition for non-rotary coating having excellent conformal properties; and to provide a method for forming a resin composition film using the composition for non-rotary coating.SOLUTION: A composition for non-rotary coating contains a resin (A) and a solvent (S). The resin (A) has a mass average molecular weight of more than 10,000. In the solvent (S), an average boiling point determined by formula:[Σ(T×R/100)] as a total sum of a product of a boiling point T(°C) of each of contained organic solvents (s), and a rate R(mass%) of each of the organic solvents (s) in the whole solvent (S) is 180°C or lower.SELECTED DRAWING: None 【課題】コンフォーマル性が良好な非回転式塗布用組成物及び当該非回転式塗布用組成物を用いる樹脂組成物膜形成方法を提供する。【解決手段】樹脂(A)及び溶剤(S)を含む、非回転式塗布用組成物であって、上記樹脂(A)は、質量平均分子量が10000超であり、上記溶剤(S)は、含有される各有機溶剤(sn)の沸点Tn(℃)と、上記各有機溶剤(sn)の上記溶剤(S)全体に占める割合Rn(質量%)との積の総和として式:[Σ(Tn×Rn/100)]で求められる平均沸点が180℃以下である、非回転式塗布用組成物。【選択図】なし
Bibliography:Application Number: JP20150036262