MOLDING METHOD OF PLATE GLASS, AND MANUFACTURING APPARATUS OF PLATE GLASS
PROBLEM TO BE SOLVED: To provide a molding method of plate glass that improves wavy deformation of a glass ribbon.SOLUTION: A molding method of plate glass includes a step for suppressing shrinkage in the width direction of a belt-like glass ribbon G. A support roll 40 is installed to support the gl...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English Japanese |
Published |
28.07.2016
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide a molding method of plate glass that improves wavy deformation of a glass ribbon.SOLUTION: A molding method of plate glass includes a step for suppressing shrinkage in the width direction of a belt-like glass ribbon G. A support roll 40 is installed to support the glass ribbon G in a viscosity range A of 10dPa s-10dPa s. The support roll 40 has at the tip a rotary member 50 that contacts the glass ribbon G, the rotary member 50 being made of ceramic without a refrigerant flow passage therein. At least part of the rotary member 50 that contacts the glass ribbon is made of sintered silicon nitride ceramic containing 0.1 mass% or less of Al, 0.7 mass% or less of Mg, 0.9 mass% or less of Ti, 3.5 mass% or less of Zr, and 0.5-10 mass% of Y.SELECTED DRAWING: Figure 1
【課題】ガラスリボンの波状の変形が改善された板ガラスの成形方法を提供する。【解決手段】帯板状のガラスリボンGの幅方向の収縮を抑制する工程を有する板ガラスの成形方法であって、前記ガラスリボンが106.7dPa・s〜107.65dPa・sの粘度範囲の領域Aで前記ガラスリボンGを支持する支持ロール40が設けられ、該支持ロール40は、前記ガラスリボンGと接触する回転部材50を先端部に有し、該回転部材50が、内部に冷媒流路を有しておらず、セラミックスで形成されている。前記回転部材50のうち少なくともガラスリボンと接触する部分が窒化ケイ素質セラミックスであり、Al:0.1質量%以下,Mg:0.7質量%以下,Ti:0.9質量%以下であり、Zr:3.5質量%以下、Y:0.5〜10質量%含有する焼結体の窒化ケイ素質セラミックスである。【選択図】図1 |
---|---|