UNDERLAYER TREATMENT SOLUTION, METHOD FOR MANUFACTURING ORGANIC COATED GALVANIZED STEEL PIPE USING THE SAME AND ORGANIC COATED GALVANIZED STEEL PIPE

PROBLEM TO BE SOLVED: To provide an underlayer treatment solution capable of forming an underlayer allowing increase of adhesion to an organic resin layer even on a galvanized layer.SOLUTION: The underlayer treatment solution comprises: an aqueous solvent; a zirconium compound having a concentration...

Full description

Saved in:
Bibliographic Details
Main Authors SUGAE KIYONOBU, KAMIMURA TAKAYUKI, KIMURA YOSHIHISA, YOSHIZAKI NOBUKI, NAKAGISHI TETSUYUKI
Format Patent
LanguageEnglish
Japanese
Published 20.06.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide an underlayer treatment solution capable of forming an underlayer allowing increase of adhesion to an organic resin layer even on a galvanized layer.SOLUTION: The underlayer treatment solution comprises: an aqueous solvent; a zirconium compound having a concentration of 0.05-10.50 mass% in terms of metal Zr; a vanadium compound having a concentration of 0.004-0.400 mass% in terms of metal V; an ammonium phosphate having a concentration of 0.07-7.50 mass% in terms of phosphate ions; a silane coupling agent having a concentration of 0.1-10 mass% in terms of a solid content and/or a hydrolytic condensate thereof; and a silica compound having a concentration of 0.2-10 mass% in terms of a solid content and has a pH of 8-12.SELECTED DRAWING: None 【課題】亜鉛めっき層上であっても、有機樹脂層の密着性を高めることができる下地層を形成可能な下地処理液を提供する。【解決手段】本実施形態の下地処理液は、水系溶媒と、金属Zr換算濃度で0.05〜10.50質量%のジルコニウム化合物と、金属V換算濃度で0.004〜0.400質量%のバナジウム化合物と、リン酸イオン換算濃度で0.07〜7.50質量%のリン酸アンモニウムと、固形分換算濃度で、0.1〜10質量%のシランカップリング剤及び/又はその加水分解縮合物と、固形分換算濃度で0.2〜10質量%のシリカ化合物とを含有し、8〜12のpHを有する。【選択図】なし