PROCESS FOR INHIBITING POLYMERIZATION OF (METH)ACRYLIC ACID AND/OR (METH)ACRYLIC ESTER

PROBLEM TO BE SOLVED: To provide a process for inhibiting polymerization of (meth)acrylic acid and/or (meth)acrylic ester.SOLUTION: The present invention provides a process for inhibiting polymerization of (meth)acrylic acid and/or (meth)acrylic ester by introducing an oxygenous gas into the (meth)a...

Full description

Saved in:
Bibliographic Details
Main Authors SCHLIEPHAKE VOLKER DR, LIPOWSKY GUNTER, RISSEL STEFFEN, HAREMZA SYLKE, JAEGER ULRICH
Format Patent
LanguageEnglish
Japanese
Published 25.02.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a process for inhibiting polymerization of (meth)acrylic acid and/or (meth)acrylic ester.SOLUTION: The present invention provides a process for inhibiting polymerization of (meth)acrylic acid and/or (meth)acrylic ester by introducing an oxygenous gas into the (meth)acrylic acid and/or the (meth)acrylic ester, in which the (meth)acrylic acid and/or the (meth)acrylic ester has a degree of purity of at least 95% and is in the liquid flocculation state.SELECTED DRAWING: None 【課題】(メタ)アクリル酸および/または(メタ)アクリル酸エステルの重合を防止する方法を提供する。【解決手段】酸素を含有するガスを、(メタ)アクリル酸および/または(メタ)アクリル酸エステルに導通することにより(メタ)アクリル酸および/または(メタ)アクリル酸エステルの重合を防止する方法であって、(メタ)アクリル酸および/または(メタ)アクリル酸エステルが、少なくとも95%の純度を有しており、かつ液状の凝集状態で存在することを特徴とする。【選択図】なし