Summary:PROBLEM TO BE SOLVED: To provide a resin molded product molded with an acrylic resin, capable of suppressing waviness after a long term storage.SOLUTION: A resin molded product 12 comprises an acrylic resin molded by an extrusion molding method or an injection molding method, and has a first external surface 12b and a second external surface 12a different from the first external surface 12b. In the first external surface 12b, the speed of water absorption is lower than the speed of water absorption in the second external surface 12a. The coefficient of water absorption is 6000-8000 ppm at the central part R1 of the first external surface 12b immediately after molded by the extrusion molding method or the injection molding method. 【課題】アクリル樹脂で成形されたものであって、長期間保管してもうねりが生じるのを抑えた樹脂成形物を提供する。【解決手段】アクリル樹脂で押出し成形法又は射出成形法で成形され、第一の外面12b及び第一の外面12bとは異なる第二の外面12aを有する樹脂成形物12であって、第一の外面12bの吸水速度は第二の外面12aの吸水速度よりも小さく、押出し成形法又は射出成形法で成形された製造直後の、第一の外面12bの中央部R1における吸水率は、6000ppm以上8000ppm以下である。【選択図】図3