METHOD FOR PRODUCING HEAT-RESISTANT ALUMINUM HYDROXIDE
PROBLEM TO BE SOLVED: To provide a method for producing aluminum hydroxide capable of withstanding the working temperature of a resin by applying high heat history while suppressing the defect and dehydration of its surface.SOLUTION: Provided is a method for producing heat-resistant aluminum hydroxi...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
09.10.2014
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide a method for producing aluminum hydroxide capable of withstanding the working temperature of a resin by applying high heat history while suppressing the defect and dehydration of its surface.SOLUTION: Provided is a method for producing heat-resistant aluminum hydroxide including heating treatment to gibbsite type aluminum hydroxide at a temperature of 180 to 300°C under the pressure of an atmospheric pressure or higher to 0.3 MPa or lower in an atmosphere satisfying a water vapor mol fraction of 0.03 to 1. |
---|---|
Bibliography: | Application Number: JP20130125733 |