MANGANESE COMPOSITE HYDROXIDE PARTICLE, POSITIVE POLE ACTIVE MATERIAL FOR NONAQUEOUS ELECTROLYTE SECONDARY BATTERY, AND NONAQUEOUS ELECTROLYTE SECONDARY BATTERY, AND METHOD FOR PRODUCING THEM
PROBLEM TO BE SOLVED: To provide a lithium/manganese composite oxide particle having a small and uniform particle size with a hollow structure; and a method for producing such a lithium/manganese composite oxide particle.SOLUTION: This manganese composite hydroxide particle is obtained through a nuc...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English |
Published |
13.12.2012
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide a lithium/manganese composite oxide particle having a small and uniform particle size with a hollow structure; and a method for producing such a lithium/manganese composite oxide particle.SOLUTION: This manganese composite hydroxide particle is obtained through a nucleation step and a particle growth step. The nucleation step is conducted such that an aqueous solution for nucleation including a metal compound containing manganese and an ammonium ion supply source is subjected to a crystallization reaction by controlling pH to be 12.0 to 14.0 based on liquid temperature of 25°C and in ambient atmosphere to generate nuclei. The particle growth step is conducted such that the aqueous solution containing nuclei formed in the nucleation step is controlled so that pH falls in the range of 10.5 to 12.0 based on liquid temperature of 25°C to be lower than that of the nucleation step, and the atmosphere is changed to an inert atmosphere within 30% of total time from the beginning of the particle growth step to grow the nuclei. The manganese composite hydroxide particle obtained in the particle growth step is mixed with a lithium compound, and the mixture is fired to obtain the lithium/manganese composite oxide particle. |
---|---|
Bibliography: | Application Number: JP20110121116 |