CONDUCTIVE MATERIAL AND TOUCH PANEL

PROBLEM TO BE SOLVED: To provide a conductive material and a touch panel which are excellent in optical transparency, conductivity, flexibility and handleability, and have an improved curling balance.SOLUTION: A conductive material comprises: a substrate; an undercoat layer and a conductive layer at...

Full description

Saved in:
Bibliographic Details
Main Authors IMAMURA KIYOBUMI, OKAZAKI KENTARO, MATSUNAMI YUKI
Format Patent
LanguageEnglish
Published 12.01.2012
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide a conductive material and a touch panel which are excellent in optical transparency, conductivity, flexibility and handleability, and have an improved curling balance.SOLUTION: A conductive material comprises: a substrate; an undercoat layer and a conductive layer at least containing conductive fibers formed in this order on one surface of the substrate; and a hard coat layer on the other surface of the substrate. The average thickness of the conductive layer is 0.01-1 μm, the average thickness of the undercoat layer is 0.1-15 μm, and the average thickness of the hard coat layer is 0.5-5 μm.
Bibliography:Application Number: JP20100142815