PROBLEM TO BE SOLVED: To provide a hard-coated antiglare film which has an extremely low haze value and antiglare properties and can prevent white blur from occurring. SOLUTION: The hard-coated antiglare film has a hard-coating antiglare layer containing fine particles on at least one surface of a t...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
21.04.2011
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To provide a hard-coated antiglare film which has an extremely low haze value and antiglare properties and can prevent white blur from occurring. SOLUTION: The hard-coated antiglare film has a hard-coating antiglare layer containing fine particles on at least one surface of a transparent plastic film substrate and a total haze value in a range of 0-5%. The number Ntotalof convexities exceeding a first standard line, which is parallel to a roughness mean line of a surface roughness profile and is located at the height of 0.1 μm, is 15 or less in a 4-mm long portion at an arbitrary location on the surface of the hard-coating antiglare layer. Ntotaland the number N50of convexities, which exceed the first standard line and have 50 μm or less length as line segments when cut at the crossings with the roughness mean line, satisfy 0.4≤N50/Ntotal≤0.8. The number of convexities, which have 50 μm or less length as line segments when cut at the crossings with the roughness mean line, among convexities exceeding a second standard line, which is parallel to the roughness mean line and is located at the height of 0.2 μm, is 10 or less. COPYRIGHT: (C)2011,JPO&INPIT |
---|---|
Bibliography: | Application Number: JP20090233938 |