OIL-RESISTANT ELASTOMER MEMBER

PROBLEM TO BE SOLVED: To provide an elastomer member which, while having a high strength, has a good balance among cold resistance, heat resistance, and rubber elasticity and also has oil resistance. SOLUTION: This oil-resistant elastomer member has a JIS A rubber hardness of 95° or lower and an elo...

Full description

Saved in:
Bibliographic Details
Main Author SHIRASAKA HITOSHI
Format Patent
LanguageEnglish
Published 30.07.2003
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:PROBLEM TO BE SOLVED: To provide an elastomer member which, while having a high strength, has a good balance among cold resistance, heat resistance, and rubber elasticity and also has oil resistance. SOLUTION: This oil-resistant elastomer member has a JIS A rubber hardness of 95° or lower and an elongation at break of 100% or higher and is resistant to a high-swelling lubricating oil. The member is prepared by cross-linking a polyester urethane prepared by the polyaddition of a polyester diol and a diisocyanate. The polyester urethane has an ester group content of 25 wt.% (5.7 mmol/g) or higher but lower than 35 wt.% (8 mmol/g) and a urethane group content of 7 wt.% (1.2 mmol/g) or higher but lower than 12 wt.% (2.0 mmol/g). COPYRIGHT: (C)2003,JPO
Bibliography:Application Number: JP20010362267