FOAMING RESTRAINING AGENT
PROBLEM TO BE SOLVED: To secure the operability of a converter comparable to the case using fluorite in the converter while restraining the foaming of slag, in the converter refining without using the fluorite. SOLUTION: A foaming restraining agent is obtained by adding and mixing, by weight ratio,...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English |
Published |
18.12.2001
|
Edition | 7 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | PROBLEM TO BE SOLVED: To secure the operability of a converter comparable to the case using fluorite in the converter while restraining the foaming of slag, in the converter refining without using the fluorite. SOLUTION: A foaming restraining agent is obtained by adding and mixing, by weight ratio, 10-5% carbon to a flux for refining containing >=80 wt.% lime powder having <=100 μm particle diameter and is formed into a pellet shape of <=50 mm by a mechanical component-pressing method. Furthermore, as the above flux for refining, the one composed of 5-20 wt.% soda glass powder and the balance substantially lime powder having <=100 μm grain size, is used. |
---|---|
Bibliography: | Application Number: JP20000170242 |