POLYETHYLENE ADHESIVE TAPE AND ITS PREPARATION PROCESS
PROBLEM TO BE SOLVED: To provide a polyethylene adhesive tape subjected to a treatment that prevents the breakage or an excessive elongation and necking, when the tape is stretched or wound. SOLUTION: The polyethylene adhesive tape, whose base material is polyethylene, is subjected to a non-necking...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English |
Published |
18.09.2001
|
Edition | 7 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Abstract | PROBLEM TO BE SOLVED: To provide a polyethylene adhesive tape subjected to a treatment that prevents the breakage or an excessive elongation and necking, when the tape is stretched or wound. SOLUTION: The polyethylene adhesive tape, whose base material is polyethylene, is subjected to a non-necking treatment on the base material to give properties (i)-(iii): (i) it has a stress at the yielding point of not less than 10 N/cm at not more than 50% of extension deformation; (ii) a deformation break occurs at 80-500% of extension deformation; and (iii) The extension stress between the yielding point and the deformation break gradually decreases with the increase in extension deformation. |
---|---|
AbstractList | PROBLEM TO BE SOLVED: To provide a polyethylene adhesive tape subjected to a treatment that prevents the breakage or an excessive elongation and necking, when the tape is stretched or wound. SOLUTION: The polyethylene adhesive tape, whose base material is polyethylene, is subjected to a non-necking treatment on the base material to give properties (i)-(iii): (i) it has a stress at the yielding point of not less than 10 N/cm at not more than 50% of extension deformation; (ii) a deformation break occurs at 80-500% of extension deformation; and (iii) The extension stress between the yielding point and the deformation break gradually decreases with the increase in extension deformation. |
Author | HIRAKAWA YONEO TANIGUCHI MASAHARU MIYATA MASAAKI |
Author_xml | – fullname: HIRAKAWA YONEO – fullname: MIYATA MASAAKI – fullname: TANIGUCHI MASAHARU |
BookMark | eNrjYmDJy89L5WQwC_D3iXQN8Yj0cfVzVXB08XAN9gxzVQhxDADy_FwUPEOCFQKCXAMcgxxDPP39gGx_Z9fgYB4G1rTEnOJUXijNzaDk5hri7KGbWpAfn1pckJicmpdaEu8VYGRgYGhkamJgauloTJQiAH5uKkM |
ContentType | Patent |
DBID | EVB |
DatabaseName | esp@cenet |
DatabaseTitleList | |
Database_xml | – sequence: 1 dbid: EVB name: esp@cenet url: http://worldwide.espacenet.com/singleLineSearch?locale=en_EP sourceTypes: Open Access Repository |
DeliveryMethod | fulltext_linktorsrc |
Discipline | Medicine Chemistry Sciences |
Edition | 7 |
ExternalDocumentID | JP2001254059A |
GroupedDBID | EVB |
ID | FETCH-epo_espacenet_JP2001254059A3 |
IEDL.DBID | EVB |
IngestDate | Fri Jul 19 12:17:51 EDT 2024 |
IsOpenAccess | true |
IsPeerReviewed | false |
IsScholarly | false |
Language | English |
LinkModel | DirectLink |
MergedId | FETCHMERGED-epo_espacenet_JP2001254059A3 |
Notes | Application Number: JP20000066227 |
OpenAccessLink | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20010918&DB=EPODOC&CC=JP&NR=2001254059A |
ParticipantIDs | epo_espacenet_JP2001254059A |
PublicationCentury | 2000 |
PublicationDate | 20010918 |
PublicationDateYYYYMMDD | 2001-09-18 |
PublicationDate_xml | – month: 09 year: 2001 text: 20010918 day: 18 |
PublicationDecade | 2000 |
PublicationYear | 2001 |
RelatedCompanies | NISHIYAMA:KK KYOWA LTD |
RelatedCompanies_xml | – name: KYOWA LTD – name: NISHIYAMA:KK |
Score | 2.5438395 |
Snippet | PROBLEM TO BE SOLVED: To provide a polyethylene adhesive tape subjected to a treatment that prevents the breakage or an excessive elongation and necking, when... |
SourceID | epo |
SourceType | Open Access Repository |
SubjectTerms | ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ADHESIVES CHEMISTRY DYES METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL PAINTS POLISHES USE OF MATERIALS AS ADHESIVES |
Title | POLYETHYLENE ADHESIVE TAPE AND ITS PREPARATION PROCESS |
URI | https://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20010918&DB=EPODOC&locale=&CC=JP&NR=2001254059A |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR1dS8Mw8JhT1DedijqVItK3YtfGfjwU6dqUrmxtcHVsT6PtUhChG67i3_farbqnvSU5OC4Hl_u-ADxxFJmUpImUawY6KJmZV0lCXUo5z-WEZ7qaVN3Io1Dz30kwfZm24LPphannhP7UwxFRojKU97J-r1f_QSy3rq1cP6cfeLR89WLLFRvvuBpzaYhu36IsciNHdBwrYGL4VsOUyjox7QM4RDtar-q_6KRftaWsdnWKdwZHDNEV5Tm0eNGBE6f5eq0Dx6NtxhuXW-FbX4DGouGMxv5sSEMq2K5Px4MJFWKb4S50hUE8FpChzN7EnXAdOcjeS3j0aOz4EhIw_7vuPGA7xKpX0C6WBb8GwczQmJHTROktDEJMxchMLecyUYmyIJnMb6C7B9HtXmgXTjfFVabUM-6gXX5983vUtmX6UHPpF9i6frA |
link.rule.ids | 230,309,783,888,25578,76884 |
linkProvider | European Patent Office |
linkToHtml | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwfR1dT4Mw8DKncb7p1EznBzGGNyKDyuCBGAZd2GTQOFy2JwKsJMaELQ7j3_dgm-5pb20vuVwvud73FeCRo8gkJImlTNPRQUmNrEwSdqWE80yOedpV47IbeeRr7jsZTp-nNfjc9sJUc0J_quGIKFEpyntRvdfL_yCWU9VWrp6SDzxavPRD0xG33nE55lIXnZ5JWeAEtmjb5pCJ_lsFU0rrxLAO4BBtbL0ctE8nvbItZbmrU_qncMQQXV6cQY3nTWjY26_XmnA82mS8cbkRvtU5aCzwZjR0Zx71qWA5Lh0PJlQILYY73xEG4VhAhjJrHXfCdWAjey_goU9D25WQgOjvutGQ7RCrXkI9X-S8BYKRojEjJ7HSmeuEGIqeGlrGZaISZU5SmV9Bew-i673Qe2i44ciLvIH_2oaTdaGVIXX0G6gXX9_8FjVvkdxVHPsF8VKBoA |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Apatent&rft.title=POLYETHYLENE+ADHESIVE+TAPE+AND+ITS+PREPARATION+PROCESS&rft.inventor=HIRAKAWA+YONEO&rft.inventor=MIYATA+MASAAKI&rft.inventor=TANIGUCHI+MASAHARU&rft.date=2001-09-18&rft.externalDBID=A&rft.externalDocID=JP2001254059A |