PROCESS FOR DECREASING OF BINDING TIME OF CHINA MORTAR AND BETONS
The starting material comprises flue-dust with Ca, water and gravel, the content of Ca(OH)2 is 2-25%. Aluminium sulphate is added in a ratio of 1 Ca(OH)2 0.75 Al2(SO4)3.