METHOD FOR MAKING MILLED ACTIVE CADMIUM TO THE PRODUCTION OF THE NEGATIVE ELECTRODE OF ALKALINE ACCUMULATOR
Cadmium metal is obtd. from a soln. of Cd salt by redn. with a more positive metal or a metal salt than Cd itself. The grain distribution is (%w/w): 5 of above 0.45 mm, 25 of 0.15-0.45 mm. The Cd salt powder is added to the reductant metal suspension comprising 0.01-50g/l PVA paste or dextrine and 1...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English |
Published |
28.07.1986
|
Edition | 4 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Cadmium metal is obtd. from a soln. of Cd salt by redn. with a more positive metal or a metal salt than Cd itself. The grain distribution is (%w/w): 5 of above 0.45 mm, 25 of 0.15-0.45 mm. The Cd salt powder is added to the reductant metal suspension comprising 0.01-50g/l PVA paste or dextrine and 1-10 -4 mol/l acid. (--pp Dwg.No.0/0) |
---|---|