PROCESS FOR THE RECOVERY OF LITHIUM

A process is divulged for the recovery of lithium from metallurgic slags comprising the steps of roasting spodumene to convert it from the alpha to the beta variant; reacting the beta variant with sulfuric acid, using a stoichiometric excess of acid; repulping the reaction product with water, formin...

Full description

Saved in:
Bibliographic Details
Main Authors DUPONT, David, OOSTERHOF, Harald
Format Patent
LanguageEnglish
Hungarian
Published 28.12.2020
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A process is divulged for the recovery of lithium from metallurgic slags comprising the steps of roasting spodumene to convert it from the alpha to the beta variant; reacting the beta variant with sulfuric acid, using a stoichiometric excess of acid; repulping the reaction product with water, forming an acidic slurry; neutralizing the acidic slurry to a pH between 5 and 7, by addition of at least one neutralizing agent; filtrating the neutralized slurry, thereby obtaining a lithium bearing solution and a residue; characterized that, in either one or both of the steps of repulping and neutralizing the acidic slurry, lithium-bearing metallurgic slag is added as neutralization agent. The lithium-bearing metallurgic slag is used to substitute at least part of the classic neutralizing agent. The lithium in the slag is released, and added to the lithium liberated from the spodumene.
Bibliography:Application Number: HUE17787424