PROCESS FOR THE PRODUCTION OF CYCLODEXTRIN POLYMERS SWELLING IN WATER QUICKLY AND TO A HIGH EXTENT
The invention relates to cyclodextrin polymers swelling quickly and to a great extent in water and a process for the preparation thereof. The cyclodextrin polymers according to the invention contain as additive n-octanol having or glycol derivative or glycerol. The cyclodextrin polymers according to...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English |
Published |
28.11.1986
|
Edition | 4 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention relates to cyclodextrin polymers swelling quickly and to a great extent in water and a process for the preparation thereof. The cyclodextrin polymers according to the invention contain as additive n-octanol having or glycol derivative or glycerol. The cyclodextrin polymers according to the invention are prepared by reacting cyclodextrin and epichlorohydrin in aqueous alkaline medium. In the reaction the cyclodextrin is reacted with 10 to 20 moles of an alkali hydroxide, 10 to 20 moles of epichlorohydrin and 2 to 8 moles of an alcohol additive, n-octanol, glycol derivative or glycerol calculated on 1 mole of cyclodextrin optionally in the presence of 10 to 15 moles of an organic solvent vaporizing at the reaction temperature or 8 to 12 moles of a high boiling organic solvent assuring heterogeneous phase. |
---|---|
Bibliography: | Application Number: HU19830000387 |