PROCESS FOR PRODUCING ANTISTATIC POLYMERIC MATERIAL

An antistatic polymeric material having surface electrical resistivity of smaller than 1010 OMEGA / &squ& order and/or half life time of shorter than 40 seconds can be obtained by heat-treating at 60-140 DEG C. for 2-60 minutes a polymeric material in a state moistened with an aqueous soluti...

Full description

Saved in:
Bibliographic Details
Main Authors SABURO HIRAOKA, SHINJI HAMA, MITSUO SENGA
Format Patent
LanguageEnglish
Published 14.06.1989
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An antistatic polymeric material having surface electrical resistivity of smaller than 1010 OMEGA / &squ& order and/or half life time of shorter than 40 seconds can be obtained by heat-treating at 60-140 DEG C. for 2-60 minutes a polymeric material in a state moistened with an aqueous solution containing 0.5-5% by weight of stannic chloride.
Bibliography:Application Number: GB19880023202