PRETREATMENT OF POLYMER SURFACES PRIOR TO PAINT COATING
The surface of a product molded of polyolefin is washed with a fluorine-containing organic solvent such as CCl2F-CCl2F or CCl2F-CClF2 and, thereafter, the product surface is treated with a plasma. Since the product surface is washed with an organic solvent containing fluorine, wastewater and process...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English |
Published |
08.06.1988
|
Edition | 4 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The surface of a product molded of polyolefin is washed with a fluorine-containing organic solvent such as CCl2F-CCl2F or CCl2F-CClF2 and, thereafter, the product surface is treated with a plasma. Since the product surface is washed with an organic solvent containing fluorine, wastewater and process operation can be controlled with relative ease. A painted product pretreated by the process of the invention has a high peel strength and water resistance. |
---|---|
Bibliography: | Application Number: GB19860007470 |