MELT BLOWING HIGHLY ORIENTED FIBERS
A thermoplastic condensation polymer is melt blown at an initial velocity of 150 to 300 m/s at a temperature which is less than 50 DEG C above its crystalline melting point and at which the molten polymer has an apparent melt viscosity of less than 50 poise. The melt blown fibers are collected to fo...
Saved in:
Main Author | |
---|---|
Format | Patent |
Language | English |
Published |
05.02.1986
|
Edition | 4 |
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A thermoplastic condensation polymer is melt blown at an initial velocity of 150 to 300 m/s at a temperature which is less than 50 DEG C above its crystalline melting point and at which the molten polymer has an apparent melt viscosity of less than 50 poise. The melt blown fibers are collected to form a non-woven web, e.g. while being contacted with hot air heating the fibers to 70-265 DEG C. A suitable apparatus is shown. |
---|---|