Melt blowing highly oriented fibers

A thermoplastic condensation polymer is melt blown at an initial velocity of 150 to 300 m/s at a temperature which is less than 50 DEG C above its crystalline melting point and at which the molten polymer has an apparent melt viscosity of less than 50 poise. The melt blown fibers are collected to fo...

Full description

Saved in:
Bibliographic Details
Main Author ECKHARD C A SCHWARZ
Format Patent
LanguageEnglish
Published 15.02.1984
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A thermoplastic condensation polymer is melt blown at an initial velocity of 150 to 300 m/s at a temperature which is less than 50 DEG C above its crystalline melting point and at which the molten polymer has an apparent melt viscosity of less than 50 poise. The melt blown fibers are collected to form a non-woven web, e.g. while being contacted with hot air heating the fibers to 70-265 DEG C. A suitable apparatus is shown.
Bibliography:Application Number: GB19830015616