PROCEDE DE SOUDAGE MIG DU NICKEL ET DES ALLIAGES DE NICKEL AVEC GAZ DE PROTECTION A BASE D'ARGON ET DE CO2

A method for the MIG welding of nickel and some nickel alloys, with a protective gas in a least a part of the welding zone, uses a protective gas containing a mixture of 0.05 to 0.5% of CO2 and argon. Advantageously, the gas mixture also contains 15 to 50% vol. and preferably 17 to 30% vol. Helium o...

Full description

Saved in:
Bibliographic Details
Main Authors FORTAIN JEAN MARIE, MOUTON JEAN YVES, BISKUP LAURENT, MARCHAND DIDIER
Format Patent
LanguageFrench
Published 18.10.2002
Edition7
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A method for the MIG welding of nickel and some nickel alloys, with a protective gas in a least a part of the welding zone, uses a protective gas containing a mixture of 0.05 to 0.5% of CO2 and argon. Advantageously, the gas mixture also contains 15 to 50% vol. and preferably 17 to 30% vol. Helium or 0.1 to 10% vol. and preferably 1 to 7% vol. Hydrogen. Independent claims are included for gas mixtures used as the protective atmosphere for the MIG welding of nickel and some nickel alloys.
Bibliography:Application Number: FR20000011349