Perfectionnements aux procédés de préparation des copolymères d'oléfines

Linear high molecular weight amorphous copolymers of ethylene with propylene or butene-1 are made by copolymerizing at a temperature of from 0 DEG to - 80 DEG C. a mixture of the monomers in the presence of a hydrocarbon solvent and a catalyst prepared at 0-80 DEG C., consisting of the reaction prod...

Full description

Saved in:
Bibliographic Details
Main Authors MAZZANTI GIORGIO, NATTA GIULIO
Format Patent
LanguageFrench
Published 21.09.1962