FLUFFMASSA OCH SAETT FOER FRAMSTAELLNING DAERAV

Improved fluffed pulp consisting of 95 to 25 percent by weight groundwood and 5 to 75 percent by weight chemical pulp, with a liquid retention capacity of at least 6.5 gram liquid per gram pulp, a liquid dispersing capacity of at least 2.5 gram liquid per gram pulp per minute, a bulk of at least 18...

Full description

Saved in:
Bibliographic Details
Main Authors AOBERG SVEN ULRIK TORBJOERN, BERGDAHL SVEN GUNNAR
Format Patent
LanguageFinnish
Published 11.04.1983
Edition3
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Improved fluffed pulp consisting of 95 to 25 percent by weight groundwood and 5 to 75 percent by weight chemical pulp, with a liquid retention capacity of at least 6.5 gram liquid per gram pulp, a liquid dispersing capacity of at least 2.5 gram liquid per gram pulp per minute, a bulk of at least 18 cm3/gram and a web strength of at least 0.2 Newton, and a method of producing said pulp by mixing 95 to 25 percent by weight groundwood and 5 to 75 percent by weight chemical pulp beaten in a wet state with each other, dewatering mechanically to a dry solids content of 40 to 50 percent by weight, coarse-defibrating, drying in a flash drying step to 60 to 85 percent by weight, finish-defibrating and finish-drying to 80 to 95 percent by weight dry solids content.
Bibliography:Application Number: FI19750003418