A hot-rolled steel strip product having a tensile strength (Rm) above 1400 MPa and a microstructure comprising at least 90 % by volume of martensite. The steel has a composition comprising, in percent by weight (wt.-%):C 0.20 - 0.26Si 0.05 - 0.5,Mn 0.2 - 0.8,Cr 0.2 - 0.6,Ni 0.2 - 0.5,Al 0.015 - 0.06...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English French German |
Published |
18.09.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A hot-rolled steel strip product having a tensile strength (Rm) above 1400 MPa and a microstructure comprising at least 90 % by volume of martensite. The steel has a composition comprising, in percent by weight (wt.-%):C 0.20 - 0.26Si 0.05 - 0.5,Mn 0.2 - 0.8,Cr 0.2 - 0.6,Ni 0.2 - 0.5,Al 0.015 - 0.065,Ti 0.005 - 0.02,B 0.001 - 0.005,optionally Cu <0.30,optionally Mo <0.10,optionally Nb <0.01,optionally V <0.04,balance Fe and unavoidable impurities. |
---|---|
Bibliography: | Application Number: EP20220818208 |