FILM STRUCTURE SUITABLE FOR RAPID LAMINATION
The invention relates to a multi-layer structure (MA) comprising: (S1) at least one first outer layer (S1) containing a polymer (P1) having a Vicat softening temperature ≥ 149°C, preferably ≥ 160°C, further preferably ≥ 170°C, more preferably ≥ 180°C, determined according to ISO 306:2004 (50N; 50°/h...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English French German |
Published |
22.05.2024
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The invention relates to a multi-layer structure (MA) comprising: (S1) at least one first outer layer (S1) containing a polymer (P1) having a Vicat softening temperature ≥ 149°C, preferably ≥ 160°C, further preferably ≥ 170°C, more preferably ≥ 180°C, determined according to ISO 306:2004 (50N; 50°/h); (S2) at least one further polymer layer (S2) containing a polymer (P2) having a Vicat softening temperature < 149°C, preferably ≤ 140°C, more preferably ≤ 130°C, determined according to ISO 306:2004 (50N; 50°/h), preferably in a range from 120 to 148°C; (S3) at least one core layer (S3); (S4) at least one further polymer layer (S4) containing a polymer (P2) having a Vicat softening temperature < 149°C, preferably ≤ 140°C, more preferably ≤ 130°C, determined according to ISO 306:2004 (50N; 50°/h), preferably in a range of 120 to 148°C; (S5) at least one second outer layer (S5) containing a polymer (P1) having a Vicat softening temperature ≥ 149°C, preferably ≥ 160°C, further preferably ≥ 170°C, more preferably ≥ 180°C, determined according to ISO 306:2004 (50N; 50°/h). The invention also relates to a method for manufacturing such a multi-layer structure and to a security document containing same. |
---|---|
Bibliography: | Application Number: EP20220747685 |