MATERIAL SYSTEMS FOR REPAIR OF THERMAL BARRIER COATING AND METHODS THEREOF

Methods for repairing a thermal barrier coating (140) deposited on a component (100) with localized spallation (150) of the thermal barrier coating (140) includes depositing a primer slurry on a thermally grown oxide (132) of the component (100) exposed by the localized spallation (150), depositing...

Full description

Saved in:
Bibliographic Details
Main Authors SAHA, Atanu, KULKARNI, Ambarish, NAGESH, Mamatha, KESHAVAN, Hrishikesh, BEWLAY, Bernard
Format Patent
LanguageEnglish
French
German
Published 13.03.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Methods for repairing a thermal barrier coating (140) deposited on a component (100) with localized spallation (150) of the thermal barrier coating (140) includes depositing a primer slurry on a thermally grown oxide (132) of the component (100) exposed by the localized spallation (150), depositing a ceramic slurry on the primer slurry, and heating the primer slurry and the ceramic slurry. The primer slurry includes a primer that includes a metal or a metal oxide. The ceramic slurry includes a ceramic material, a ceramic slurry binder material, and a ceramic slurry fluid carrier. Heating the primer slurry and the ceramic slurry forms a first chemical bond (210) between the primer and the thermally grown oxide (132) and a second chemical bond (230) between the primer and the ceramic material.
Bibliography:Application Number: EP20230195249