SHEAR THINNING THERMALLY CONDUCTIVE SILICONE COMPOSITIONS

A composition contains the following components: (a) 15 to 49.8 volume-percent of a first polysiloxane that is has a viscosity in a range of 50 centiStokes to 550 Stokes as determined according to ASTM D4283-98; (b) 0.2 to 5 volume-percent of an organoclay; (c) 50-74 volume-percent roundish or crush...

Full description

Saved in:
Bibliographic Details
Main Authors FRANKEL, Erica A, BECERRA, Andrés E, SWARTZ, Andrew J, HANSEN, Darren
Format Patent
LanguageEnglish
French
German
Published 10.01.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A composition contains the following components: (a) 15 to 49.8 volume-percent of a first polysiloxane that is has a viscosity in a range of 50 centiStokes to 550 Stokes as determined according to ASTM D4283-98; (b) 0.2 to 5 volume-percent of an organoclay; (c) 50-74 volume-percent roundish or crushed thermally conductive fillers including: (i) 5 to 15 volume-percent small thermally conductive fillers having a median particle size in a range of 0.1 to 1.0 micrometers; (ii) 10 to 25 volume-percent medium thermally conductive fillers having a median particle size in a range of 1.1 to 5.0 micrometers; (iii) 25 to 50 volume-percent large thermally conductive fillers having a median particle size in a range of 5.1 to 50 micrometers; and (d) 0 to 5 volume-percent of an alkoxy functional linear polysiloxane different from the first polysiloxane and/or an alkoxy functional linear silane; where volume-percent values are relative to composition volume.
Bibliography:Application Number: EP20210710689