POLYOLEFIN MICROPOROUS MEMBRANE
Provided is a polyolefin microporous membrane containing polyethylene, wherein the melting peak of nonrev. heat flow measured by a temperature-modulated DSC method at a temperature rise rate of 1°C/min of the polyolefin microporous membrane is within the range of 141.0°C to 150.0°C.
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English French German |
Published |
27.04.2022
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Provided is a polyolefin microporous membrane containing polyethylene, wherein the melting peak of nonrev. heat flow measured by a temperature-modulated DSC method at a temperature rise rate of 1°C/min of the polyolefin microporous membrane is within the range of 141.0°C to 150.0°C. |
---|---|