PRODUCTION METHOD FOR CEMENT CLINKER AND CEMENT CLINKER POWDER

Portland cement clinker that includes C3A and C4AF in total from 22 to 40 mass % calculated by Bogue's formulas and has an iron modulus (I.M.) of 0.8 to 1.3 is produced. The burned raw materials are annealed at a cooling rate of 20 degree Celsius or lower at least to 1200 degree Celsius so that...

Full description

Saved in:
Bibliographic Details
Main Authors MORI, Akiyoshi, CHABAYASHI, Takashi
Format Patent
LanguageEnglish
French
German
Published 28.12.2022
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:Portland cement clinker that includes C3A and C4AF in total from 22 to 40 mass % calculated by Bogue's formulas and has an iron modulus (I.M.) of 0.8 to 1.3 is produced. The burned raw materials are annealed at a cooling rate of 20 degree Celsius or lower at least to 1200 degree Celsius so that the lightness of the cement clinker is made high. When annealing till lower temperatures, the lightness value becomes generally higher, but the effect becomes negligible lower at 1000 degree Celsius. Therefore, the raw materials are quenched at 1000 degree Celsius and lower for improving the productiveness.
Bibliography:Application Number: EP20200775808