PROCESS FOR MAKING A MIXED METAL OXIDE
A process for making a mixed metal oxide, may involve: (a) providing a hydroxide or oxyhydroxide of TM with an average particle diameter (D50) in the range of from 0.1 μm to 5 mm; (b) subjecting the hydroxide or oxyhydroxide of TM to a stream of gas with a temperature in the range of from 150 to 200...
Saved in:
Main Authors | , |
---|---|
Format | Patent |
Language | English French German |
Published |
17.02.2021
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | A process for making a mixed metal oxide, may involve: (a) providing a hydroxide or oxyhydroxide of TM with an average particle diameter (D50) in the range of from 0.1 μm to 5 mm; (b) subjecting the hydroxide or oxyhydroxide of TM to a stream of gas with a temperature in the range of from 150 to 2000° C., wherein TM contains nickel and at least one further transition metal selected from cobalt and manganese. |
---|---|
Bibliography: | Application Number: EP20190711110 |