METHOD FOR PRODUCING TEMPERATURE-STABLE POLYALKENAMERS
The polymerization of cycloalkenamer is stopped by adding an alkyl vinyl derivative. Subsequently compound A is added, wherein compound A has at least one of the features i) or ii): i) at least one functional group or ii) at least one saturated or unsaturated aliphatic or aromatic heterocyclic ring...
Saved in:
Main Authors | , , , |
---|---|
Format | Patent |
Language | English French German |
Published |
08.07.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | The polymerization of cycloalkenamer is stopped by adding an alkyl vinyl derivative. Subsequently compound A is added, wherein compound A has at least one of the features i) or ii): i) at least one functional group or ii) at least one saturated or unsaturated aliphatic or aromatic heterocyclic ring having 3 to 14 ring atoms, wherein the ring atoms contain at least one carbon atom and at least one atom selected from oxygen, nitrogen and sulfur. A membrane filtration is subsequently carried out. This type of production produces polyalkenamers which are temperature-stable at 180° C. |
---|---|
Bibliography: | Application Number: EP20190712814 |