THERMOPLASTIC POLYOLEFIN BLENDS INCLUDING BLOCK COMPOSITES AS COMPATIBILIZERS

A composition comprising (A) from 10 wt% to 90 wt% of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt%, based on the total weight of the propylene based polymer, and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min (ASTM D-1238...

Full description

Saved in:
Bibliographic Details
Main Authors HENSCHKE, Olaf, JELTSCH, Krischan, OHMURA, Takahiko, MING, Ming, ZHANG, Yahong, WU, Hang, LI, Wei, HU, Yushan
Format Patent
LanguageEnglish
French
German
Published 20.03.2024
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A composition comprising (A) from 10 wt% to 90 wt% of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt%, based on the total weight of the propylene based polymer, and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min (ASTM D-1238 at 230°C, 2.16 kg); (B) from 1 wt% to 60 wt% of a polyolefin elastomer; (C) from 1 wt% to 20 wt% of a block composite comprising (i) an ethylene-propylene copolymer, (ii) an isotactic polypropylene copolymer, and (iii) a block copolymer including an ethylene-propylene soft block that has a same composition as the ethylene-propylene copolymer of the block composite and an isotactic polypropylene hard block that has a same composition as the isotactic polypropylene copolymer of the block composite; and (D) optionally, from 0.1 wt% to 10 wt% of an antioxidant.
Bibliography:Application Number: EP20170728373