LAMINATED GLASS ARTICLE WITH APERTURE FORMED THEREIN AND METHODS FOR FORMING THE SAME

A glass article (100) includes a core layer (102) formed from a core glass composition with a core coefficient of thermal expansion (CTE) and first (104) and second (106) cladding layers fused to first and second major surfaces of the core layer (102) and formed from a clad glass composition compris...

Full description

Saved in:
Bibliographic Details
Main Authors SPRING, Kevin Eugene, SUBRAMANIAN, Vijay, SHAFRIR, Shai Negev, BURNETT, David Aaron
Format Patent
LanguageEnglish
French
German
Published 30.01.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A glass article (100) includes a core layer (102) formed from a core glass composition with a core coefficient of thermal expansion (CTE) and first (104) and second (106) cladding layers fused to first and second major surfaces of the core layer (102) and formed from a clad glass composition comprising a clad CTE. An aperture (120) extends through each of the core layer (102), the first cladding layer (104), and the second cladding layer (106). The clad CTE is less than the core CTE such that each of the first (104) and second (106) cladding layers is under a compressive stress and the core layer (102) is under a tensile stress. A flexural strength of the glass article (100) can be at least about 75 MPa. A peak load sustainable by the glass article (100) in a modified ring-on-ring test can be at most 96.5% less than a peak load sustainable by a reference glass article in the modified ring-on-ring test.
Bibliography:Application Number: EP20170715617