FERRITIC-AUSTENITIC TWO-PHASE STAINLESS STEEL MATERIAL AND METHOD FOR MANUFACTURING SAME

A steel material contains, in mass%, C: 0.005 to 0.050, N: 0.05 to 0.30, Si: 0.1 to 1.5, Mn: 0.1 to 7.0, P: 0.005 to 0.100, S: 0.0001 to 0.0200, Cr: 18.0 to 28.0, Cu: 0.1 to 3.0, Ni: 0.1 to 8.0, Mo: 0.1 to 5.0, Al: 0.001 to 0.050, B: 0.0001 to 0.0200, and Ca: 0.0001 to 0.0100. An area ratio of an au...

Full description

Saved in:
Bibliographic Details
Main Authors HIRAIDE Nobuhiko, HAYASHI Atsutaka, HAMADA Junichi
Format Patent
LanguageEnglish
French
German
Published 03.07.2019
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A steel material contains, in mass%, C: 0.005 to 0.050, N: 0.05 to 0.30, Si: 0.1 to 1.5, Mn: 0.1 to 7.0, P: 0.005 to 0.100, S: 0.0001 to 0.0200, Cr: 18.0 to 28.0, Cu: 0.1 to 3.0, Ni: 0.1 to 8.0, Mo: 0.1 to 5.0, Al: 0.001 to 0.050, B: 0.0001 to 0.0200, and Ca: 0.0001 to 0.0100. An area ratio of an austenitic phase ranges from 30% to 70% and formulae (I) and (II) below are satisfied. 1.03 ‰¤ % Cr * F / % Cr ‰¤ 1.40 1.05 ‰¤ % Mn * A / % Mn ‰¤ 1.80 [% symbol of an element]: a content of the element in the steel [% symbol of an element*F]: a content of the element in a ferrite phase [% symbol of element*A]: a content of the element in the austenitic phase
Bibliography:Application Number: EP20170753164