POLYMERS WITH IMPROVED ESCR FOR BLOW MOLDING APPLICATIONS
Disclosed herein are ethylene-based polymers generally characterized by a density greater than 0.954 g/cm3, high load melt index ranging from 10 to 45 g/10 min, a ratio of high load melt index to melt index ranging from 175 to 600, a rheological slope parameter ranging from 0.15 to 0.30, and an ESCR...
Saved in:
Main Authors | , , , , |
---|---|
Format | Patent |
Language | English French German |
Published |
11.03.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Disclosed herein are ethylene-based polymers generally characterized by a density greater than 0.954 g/cm3, high load melt index ranging from 10 to 45 g/10 min, a ratio of high load melt index to melt index ranging from 175 to 600, a rheological slope parameter ranging from 0.15 to 0.30, and an ESCR in 10% igepal exceeding 800 hours. These polymers have the beneficial processability and die swell features of chromium-based resins, but with improved stiffness and stress crack resistance, and can be used in blow molding and other end-use applications. |
---|---|
Bibliography: | Application Number: EP20160767425 |