POLYPROPYLENE COMPOSITION WITH EXCELLENT PAINT ADHESION

The invention relates to a polypropylene composition (C) comprising: (i) 62 to 85 wt.-%, based on the total weight of the polypropylene composition (C), of a heterophasic propylene copolymer (HECO1) with a melt flow rate MFR 2 (230 °C) measured according to ISO 1133 in the range of 6.0 to 50.0 g/10m...

Full description

Saved in:
Bibliographic Details
Main Authors SHUTOV, Pavel, KNIESEL, Claudia, MILEVA, Daniela, PRADES, Floran, KAHLEN, Susanne
Format Patent
LanguageEnglish
French
German
Published 07.06.2023
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:The invention relates to a polypropylene composition (C) comprising: (i) 62 to 85 wt.-%, based on the total weight of the polypropylene composition (C), of a heterophasic propylene copolymer (HECO1) with a melt flow rate MFR 2 (230 °C) measured according to ISO 1133 in the range of 6.0 to 50.0 g/10min; (ii) 10 to 30 wt.-%, based on the total weight of the polypropylene composition (C), of a heterophasic propylene copolymer (HECO2) with a melt flow rate MFR 2 (230 °C) measured according to ISO 1133 in the range of 0.1 to 5.5 g/10min; (iii) 5 to 30 wt.-%, based on the total weight of the polypropylene composition (C), of an inorganic filler (F); wherein (a) the xylene cold soluble (XCS) fraction of the heterophasic propylene copolymer (HECO1) has a lower amount [in mol%] of C 2 and/or C 4 to C 12 ±-olefin derived comonomer units than the xylene cold soluble (XCS) fraction of the heterophasic propylene copolymer (HECO2); (b) the xylene cold soluble (XCS) fraction of the heterophasic propylene copolymer (HECO1) has a lower the intrinsic viscosity (IV) than the xylene cold soluble (XCS) fraction of the heterophasic propylene copolymer (HECO2); and (c) the xylene cold soluble (XCS) fraction of the heterophasic propylene copolymer (HECO2) has an intrinsic viscosity (IV) in the range of 6.0 to 15.0 dl/g.
Bibliography:Application Number: EP20160204510