R-(FE,CO)-B SINTERED MAGNET AND MAKING METHOD

An R-(Fe,Co)-B base sintered magnet consisting essentially of 12-17 at% of R containing Nd and Pr, 0.1-3 at% of M 1 (typically Si), 0.05-0.5 at% of M 2 (typically Ti), B, and the balance of Fe, and containing R 2 (Fe,Co) 14 B as a main phase has a coercivity of at least 10 kOe. The magnet contains a...

Full description

Saved in:
Bibliographic Details
Main Authors HIROTA, Koichi, HASHIMOTO, Takahiro, NAKAMURA, Hajime, KAMATA, Masayuki
Format Patent
LanguageEnglish
French
German
Published 28.04.2021
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:An R-(Fe,Co)-B base sintered magnet consisting essentially of 12-17 at% of R containing Nd and Pr, 0.1-3 at% of M 1 (typically Si), 0.05-0.5 at% of M 2 (typically Ti), B, and the balance of Fe, and containing R 2 (Fe,Co) 14 B as a main phase has a coercivity of at least 10 kOe. The magnet contains a M 2 boride phase at a grain boundary triple junction, and has a core/shell structure that the main phase is covered with a grain boundary phase. The grain boundary phase is composed of an amorphous and/or nanocrystalline R'-(Fe,Co)-M 1 ' phase consisting essentially of 25-35 at% of R' containing Pr, 2-8 at% of M 1 ' (typically Si), up to 8 at% of Co, and the balance of Fe. A coverage of the main phase with the R'-(Fe,Co)-M 1 ' phase is at least 50%, and the bi-granular grain boundary phase has a width of at least 50 nm.
Bibliography:Application Number: EP20160198513