METHOD FOR SMELTING NICKEL OXIDE ORE
Provided is a method for smelting nickel oxide ore by which the occurrence of cracking due to heat shock can be suppressed when nickel oxide ore is pelletized and charged into a smelting step (reduction step). A method for smelting nickel oxide ore according to the present invention uses pellets of...
Saved in:
Main Authors | , , |
---|---|
Format | Patent |
Language | English French German |
Published |
04.03.2020
|
Subjects | |
Online Access | Get full text |
Cover
Loading…
Summary: | Provided is a method for smelting nickel oxide ore by which the occurrence of cracking due to heat shock can be suppressed when nickel oxide ore is pelletized and charged into a smelting step (reduction step). A method for smelting nickel oxide ore according to the present invention uses pellets of nickel oxide ore, the method being characterized by comprising a pellet production step S1 for producing pellets from nickel oxide ore, and a reduction step S2 for heating the resulting pellets at a predetermined reduction temperature in a reduction furnace, the reduction step S2 comprising preheating the pellets obtained in the pellet production step S1 to a temperature of 350 to 600°C in the reduction furnace and thereafter charging the pellets into the reduction furnace and raising the temperature of the reduction furnace to the reduction temperature. |
---|---|
Bibliography: | Application Number: EP20150828220 |