MINERAL FILLED POLYPROPYLENE COMPOSITION

A polypropylene composition for the production of molded articles, such as finished parts for the automotive industry, has melt flow rate (230°C, 2.16 Kg) of at least 25 g /10 min and comprises: (A) 50-95% of a composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C of 3...

Full description

Saved in:
Bibliographic Details
Main Authors WILLEMS, SANDER, CIARAFONI, MARCO, MASSARI, PAOLA, ROHRMANN, JÜRGEN
Format Patent
LanguageEnglish
French
German
Published 26.10.2016
Subjects
Online AccessGet full text

Cover

Loading…
More Information
Summary:A polypropylene composition for the production of molded articles, such as finished parts for the automotive industry, has melt flow rate (230°C, 2.16 Kg) of at least 25 g /10 min and comprises: (A) 50-95% of a composition having an intrinsic viscosity of the fraction soluble in xylene at 25 °C of 3.0-5.0 dl/g and comprising: (Al) 70-95% of a propylene homopolymer having a Polydispersity Index (PI) of 4.3-10, a fraction insoluble in xylene at 25 °C higher than 90% and a MFR (230°C, 2.16 Kg) of 100- 250 g/10 min; (A2) 5-30% of a copolymer of propylene with 36-44% of ethylene-derived units; (B) optionally up to 45% of a heterophasic propylene polymer, having MFR (230°C, 2.16 Kg) of 10-25 g/10 min, flexural modulus higher than 1400 MPa, and comprising 5-20% of a copolymer rubber component and 80-95% of a matrix propylene polymer component; (C) 2-10% of an ethylene based elastoplastic copolymer; and (D) optionally up to 20% of talc.
Bibliography:Application Number: EP20140821562